'Using fractional elements, it is possible to finely control the compounding process to a great extent'
Co-rotating twin-screw extruders have evolved through the years. Deeper flights lead to increased
efficiencies and reduced shear rates in a twin-screw extruder. This feature is advantageous in
increasing the screw speed thereby maintaining mixing rates and increasing the volumetric capacity of
the machine. An improvement in process efficiency is realized due to the reduction in viscous dissipation
per unit mass of material. The ability to process material has benefited from improvements made in diameter
ratio and specific torque. The advantages with deeper screw flights are higher intake capacity (especially
in starve feed), lower melt temperature due to decreased shear stress, and greater devolatisation capacity.
Further, the ability to process certain shear and temperature sensitive materials is greatly enhanced in an
extruder with deeper flights.
The increase in melt temperature due to the kneading elements at high speeds is solved by fractional
lobed element geometry with unequal tip angles. This geometry can easily replace standard kneading elements.
Forty years ago, Erdmenger determined the need for fractional elements. Erdmenger said, �One disadvantage that was
hitherto encountered in apparatuses of this type (twin-screw extruders) was that it was only possible to vary the
dimension lying in the axial direction but not the dimension lying transversely to the axis, e.g. the thickness of
the layer of material used, which often has an important effect on the transfer of heat or the transfer of material
or the course of the reaction, which in practice is the most important alteration"
The standard twin-screw elements have equal tip angles for all lobes. These limit the types of elements that operate
in a twin-screw extruder if the geometry is based solely on the design of Erdmenger. For example, in an eccentric
trilobed kneading element, the small tip angle leads to higher wear rate. Increasing the tip-angle gives a circular
shape to the element and reduces the free volume available in the extruder. Elements having different tip-angles have
been invented by Dr. Babu Padmanabhan. These elements continue to work as conjugate pairs while suiting the needs of
twin-screw extrusion. The new element geometry provides greater flexibility in design of individual elements.
The end profile of a fractional element formed as a result of transforming a one-lobe to a four-lobe profile as shown in Figure 1.
This shows the profile at a location that is halfway through the transformation. At every step of the transformation the
profile obtained has to be intermeshing and fully wiping.
Figure 2 clearly shows the basis for the classification.
The last two digits provide the location of the transformation from one lobe to two-lobe profile. If 'n' is the number
of lobes on one end with less lobes and �N� is the number of lobes on the other end with more lobes, then the condition
for perfect transformation is that �N/n� should be a whole number.
Figure 3 shows the configuration of the extruder screw
where the regular kneading blocks are formed with fractional lobed geometry. The screw speed and configuration are the two
key variables. The zone temperatures are shown on the barrel segments. The kneading length in the mixing zone of both the
configuration are maintained at 180mm and also increase in pressure matches both configuration. The fractional lobed geometry
shown in this configuration is selected based on certain observations made on the changes in cross-section during rotation of
the corresponding geometry. The motivation was to avoid high pressure points during the full 360 degree turn of the flights.
'Elements having different tip angles continue to work as conjugate pairs, while suiting the needs of twin-screw extruder�


Plant: Steer ADC |
Extruder: Omega 40 |
Shaft Length |
Diameter : 39.7 mm |
Line Code: ADC2 |
Author: Dr. Babu |
Max: RPM : 600 |
Offset : 0 mm |
Configuration Code: LLDPE Tie2 Fr |
Revision Number: 0 |
Max: KW : 70 |
|
Figure 3: Configuration with Fractional Kneading Blocks
Processing on various materials with fractional-lobed elements has already been carried out. This involved processing
of polymers with a high filling of carbon black, organic pigments, glass fibre, etc. Fractional elements were also
used on PVC compounding. Using fractional elements, it is possible to finely control the compounding process to a
greater extent than what is considered possible with standard elements.
This article is contributed by Dr. Babu Padmanabhan, Managing Director and Founder of Steer Engineering. He is
a PHD in Mechanical Engineering from Virginia Polytechnic Institute and State University Blacksburg VA.
|
{{comment.DateTimeStampDisplay}}
{{comment.Comments}}