Technical Papers Plastics
Ultrasonic cleaning is the best method for cleaning dies and moulds

Ultrasonic cleaning is the best method for cleaning dies and moulds

Techno - commercial information on plastics Industry - News on Plastics Industry - Plastemart.com
 
Ultrasonic cleaning is the best method for cleaning dies & moulds
Ultrasonic cleaning is the best method for cleaning dies and moulds  
 

Cleaning dies and moulds is labour intensive and also often abrasive. By using ultrasonics for mould maintenance, the result is a cleaner mould with reduced manual input and no wear leading to large cost savings, extended mould life, and shorter payback time. The technique suits plastic, rubber and die cast moulds and tools.
Ultrasonic cleaning uses high-frequency sound waves to remove mould residues and fouling from tooling and plates that are immersed in a heated (usually 80 degree C) aqueous solution. An ultrasonic generator converts standard line-frequency current (60 or 50 Hz) into high-frequency electrical energy (20,000 Hz or more). The generator is connected to small transducers that are mounted to the bottom or sides of a wash tank. These transducers vibrate at ultrasonic frequencies (20 kHz and above) when the current passes through. This causes the bottom or sides of the tank to vibrate like the diaphragm in a speaker, which creates microscopic bubbles that form and collapse in the tank (a phenomenon known as cavitation), which scrub and loosen vent residues and grime. The energy released from these microscopic scrubbing bubbles produces forces at 10,000 degree F at 7500 psi, which is powerful enough to loosen contaminants without damaging critical edges or surface finishes.

Ultrasonic cleaning gives the following advantages:

Short wash process leading to reduced time spent in cleaning
No manual labour required. An operator is not required when the machine is cleaning the mould
High levels of cleanliness give longer life in production
No abrasion of precise edges and surfaces gives longer mould life
No solvents needed because of aqueous process
Suitable for all moulds, large and small
Machinery is simple and easy to use
The ultrasonic cleaning of molding equipment, such as injection molds and blow molds, will require the same three processing stages as any other type product when cleaned with aqueous cleaning agents; the Ultrasonic Cleaning Stage, where contaminants are removed from the product, the Rinsing Stage, where the detergent residues are removed from the product, and the Drying Stage, where rinse water is removed from the product. Although the 3 main stages are the same, the ultrasonic cleaner must be properly configured with additional equipment to clean these items successfully.

Most molding equipment is composed of a number of different metals, which may include steel, stainless steel, brass, aluminum, and exotic metals. Therefore, the cleaning fluid selected must be multi-metal compatible. This makes the cleaning of these items a bit more difficult, since most cleaning agents which are compatible with aluminum are rather gentle, and can not loosen the contamination as well as cleaners which are more aggressive. Since steel is typically included, the ultrasonic cleaner must also include a Rust Preventative stage after the final rinse.
The cleaning ability of ultrasonic depends on several key factors, of which the cleaning solution is the most important variable. The type of detergent required is dependent upon the process and type of resin, which leaves behind specific types of off-gassing residue. Highly alkaline solutions such as sodium hydroxide do the best job of removing stubborn contaminants, light rust and heavy grease on most tooling and plates, with no harm to most plating and coatings. On the downside- it can be caustic, posing a potential health risk, and may require neutralization before disposal.
Mild alkaline solutions also are available that perform well on many residues without the caustic issues. But in general, the friendlier the detergent, the less effective it will be on stubborn contaminants.
Slightly acidic solutions, such as those containing low concentrations of citric acid, excel at rust and oxide removal, but must be used with caution on some tool steels because they can react with the iron in the steel, turning it gray. This normally does not cause a technical problem but doesn't sit well with toolmakers.

Another difficulty involves the complex design of the molding equipment being cleaned. Most molds include a large number of internal channels which are used to release gasses during the molding process. In order the effectively clean inside of these holes, these areas must be filled with liquid during the ultrasonic cleaning process. This may require that parts be submerged in a particular orientation, or perhaps the item must be rotated once submerged to fill these areas with cleaning agent, and allow the ultrasonic cleaner to effectively cavitate inside of these critical areas. However, these areas must also drain properly prior to entering the rinse cycle and the drying cycle, or the dirt which has been loosened during the ultrasonic cleaning stage will remain trapped within the part.

Most molding equipment is also very heavy and dense. These items tend to absorb a significant amount of ultrasonic energy, and the ultrasonic cleaner must include a higher power level than an ultrasonic cleaner designed to remove oils from sheetmetal parts. The ultrasonic cleaner must also include the proper ultrasonic frequencies to provide the fastest and most consistent cleaning results.

 
 
  Back to Articles

Previous Article

Next Article

COMMENTS

0

*

Email Id Required.

Email Id Not Valid.

*

Mobile Required.

*

Name Required.

*

Please enter Company Name.

*

Please Select Country.

Email ID and Mobile Number are kept private and will not be shown publicly.
*

Message Required.

Click to Change image  Refresh Captcha
Unused tiffin, lunch box moulds

Unused tiffin, lunch box moulds